Thixotropic cementitious mortar with PAN fibres – STRUTTURA TIXO – TX 376

Pre-mixed, single-component, thixotropic, shrinkage-compensated cementitious mortar, fibre-reinforced with synthetic fibres, for repairing, restoring or reinforcing deteriorated concrete, reinforced concrete and masonry structures, applied, depending on the thickness to be treated, to substrates prepared with hydro-scarification or sandblasted surfaces. Medium thickness work from 10 mm to 50 mm.

TX376-25 :

25 kg bag – PACKAGE/PALLET: 60

CE STRUTTURA EN 1504-3 R4 AVCP 2+

Strength class

60MPa

Matching price codes

codes ANAS

B.09.220.2 B.09.220.2.a B.09.220.2.b

codes ASPI

MT2

Technical data

PARTICLE SIZE
AVERAGE CONSUMPTION
MIXING WATER (% BY MASS)
MIXTURE LIFESPAN
COMPRESSIVE STRENGTH (28 DAYS)
≤ 3 mm
18,6 kg per m² per cm of thickness
14-16 % (3,50-4,00 L Per 25 kg bag)
60 min
60 MPa

SHARE

Share Facebook Share Linkedin Share Mail Whatsapp

References and related technical articles

Concrete restoration works for the Atrani bridge

Case History

Concrete restoration works for the Atrani bridge

InfrastructureBridges and Viaducts

Certifications

Associations