Thixotropic cementitious mortar polymer modified – STRUTTURA TIXO – TX 259

Thixotropic, premixed, polymer modified, single-component, shrinkage-compensated cementitious mortar, fibre-reinforced with synthetic fibres, weather-resistant. Applicable in thickness from 10 mm to 50 mm. Suitable for cortical restoration of degraded concrete and reinforced concrete structures.

TX259-25 :

25 kg bag – PACKAGE/PALLET: 60

TX259-SRA :

25 kg bag – PACKAGE/PALLET: 60

CE STRUTTURA EN 1504-3 R4 AVCP 2+

Strength class

50MPa

Matching price codes

codes ANAS

B.09.220.1 B.09.220.1.a B.09.220.1.b (monocomponente)

codes ASPI

MT3 (monocomponente)

Technical data

PARTICLE SIZE
AVERAGE CONSUMPTION
MIXING WATER (% BY MASS)
MIXTURE LIFESPAN
COMPRESSIVE STRENGTH (28 DAYS)
≤ 3 mm
18,4 kg per m² per cm of thickness
15-17% (3,75-4,25 L Per 25 kg bag)
60 min
50 MPa